Bio-based polyester-polyurethane foams: synthesis and degradability by Aspergillus niger and Aspergillus clavatus
; Russell White, Karen ; Vaillard, Santiago Eduardo
; Ríos, Luis
; Meira, Gregorio Raul
; Estenoz, Diana Alejandra
; Spontón, Marisa Elisabet 
Otros responsables
Fecha
11/2023
Editorial
Springer
Revista
Biodegradation
Título del libro
Nombre del evento
Fecha del evento
Institución organizadora
ISSN
0923-9820
eISSN
ISBN
Idioma
Inglés
Tipo del evento
Clasificación temática
Palabras clave
Resumen
In this article, the degradability by Aspergillus niger and Aspergillus clavatus of three bio-based polyurethane (PU) foams is compared to previous degradability studies involving a Pseudomonas sp. bacterium and similar initial materials (Spontón et al. in Int. Biodet. Biodeg. 85:85–94, 2013, https://doi.org/10.1016/j.ibiod.2013.05.019). First, three new polyester-polyurethane foams were prepared from mixtures of castor oil (CO), maleated castor oil (MACO), toluene diisocyanate (TDI), and water. Then, their degradation tests were carried out in an aqueous medium, and employing the two mentioned fungi, after their isolation from the environment. From the degradation tests, the following was observed: (a) the insoluble (and slightly collapsed) foams exhibited free hydroxyl, carboxyl, and amine moieties; and (b) the water soluble (and low molar mass) compounds contained amines, carboxylic acids, and glycerol. The most degraded foam contained the highest amount of MACO, and therefore the highest concentration of hydrolytic bonds. A basic biodegradation mechanism was proposed that involves hydrolysis and oxidation reactions. Graphical abstract: [Figure not available: see fulltext.].