Lowering the synthesis temperature of high-purity BaTiO3 powders by modifications in the processing conditions

Otros responsables
Fecha
03/2003
Editorial
Elsevier Science
Revista
Thermochimica Acta
Título del libro
Nombre del evento
Fecha del evento
Institución organizadora
ISSN
0040-6031
eISSN
ISBN
Idioma
Inglés
Tipo del evento
Clasificación temática
Palabras clave
Resumen
In this work, the influence of the BaCO3:TiO2 ratio and milling conditions on the solid-state barium titanate formation at high temperature has been studied. An excess of TiO2 improved the BaTiO3 formation when the TiO2 reactivity was low. Besides, long milling time and an excess of fine grained titanium led to agglomerate formation. In addition, mechanochemical activation performed by rigorous milling and the employment of fine particles of anatase-rich TiO2 powder allowed the reaction to go to completions at temperatures about 150 °C and below than traditionally need.
Colecciones
Aprobación
Revisión
Complementado por
Referenciado por
Licencia Creative Commons
Excepto donde se indique lo contrario, la licencia de este ítem se describe como by-nc-nd