Intrinsic Kinetics of Chlorination of WO3 Particles With Cl2 Gas Between 973 K and 1223 K (700 °C and 950 °C)
; Bohe, Ana Ester
; Sohn, H. Y. Otros responsables
Fecha
12/2010
Editorial
Springer
Revista
Metallurgical And Materials Transactions B-process Metallurgy And Materials Processing Science
Título del libro
Nombre del evento
Fecha del evento
Institución organizadora
ISSN
1073-5615
eISSN
ISBN
Idioma
Inglés
Tipo del evento
Clasificación temática
Palabras clave
Resumen
Chlorination is one of the methods applied in extractive metallurgy for the treatment of mineralsto obtain valuable metals, such as titanium and zirconium. The possibility of applying chlori-nation metallurgy to other metals such as tungsten was the major aim of this study. The kineticsof the chlorination of tungsten oxide (WO3) particles has been investigated by thermogravimetrybetween 973 K and 1223 K (700 C and 950 C) and for partial pressures of chlorine rangingfrom 15 to 70 kPa. The starting temperature for the reaction ofWO3 with chlorine is determinedto be about 920 K (647 C). The influence of chlorine diffusion through the bulk gas phase andthrough the particle interstices in the overall rate was analyzed. In the absence of these twomass-transfer steps, a reaction order of 0.5 with respect to chlorine partial pressure, and anactivation energy of 183 kJ/mol were determined. For tungsten oxide particles of less than50-lm size, a complete rate expression has been obtained.