Alkali-silica reaction in mortars and concretes incorporating natural rice husk ash
; Giaccio, Graciela Marta ; Batic, O. R. ; Isaia, G. C. Otros responsables
Fecha
11/2012
Editorial
Elsevier
Revista
Construction And Building Materials
Título del libro
Nombre del evento
Fecha del evento
Institución organizadora
ISSN
0950-0618
eISSN
ISBN
Idioma
Inglés
Tipo del evento
Clasificación temática
Palabras clave
Resumen
Rice-husk ash (RHA) is a supplementary cementing material of great interest in many developing countries. Before using in concrete the rice husk needs to be burnt at a controlled temperature. In other conditions a residual RHA is obtained with a lower quality, but it can be improved by grinding (GRHA). As a way to simplify RHA processing and amplify its use nearby where it is produced, it was demonstrated that it is possible to produce structural concretes incorporating residual RHA "as nature" (NRHA), adapting the mixing process to optimize the ash particle size by grinding it in the mixer together with the coarse aggregate. Nevertheless as RHA has siliceous vitreous minerals and cristobalite, deleterious reactions with Portland cement can take place when alkalis and certain environmental conditions are present. This paper studies the development of alkali-silica reaction (ASR) in mortars and concretes prepared with NRHA and GRHA. Accelerated and long term expansion tests, mechanical characterization, microscopic observations and studies on prototypes are included. The RHA can inhibit or promote ASR depending on its particle size. Furthermore, the risks of cracking and the selection criteria for the best binders when using NRHA are shown.
Colecciones
Aprobación
Revisión
Complementado por
Referenciado por
Licencia Creative Commons
Excepto donde se indique lo contrario, la licencia de este ítem se describe como by-nc-sa