Artículo
Intrinsic Kinetics of the Chlorination of RuO2 with Cl2 Between 973 K and 1073 K (700 °C and 800 °C)
Fecha de publicación:
30/04/2016
Editorial:
Springer
Revista:
Metallurgical And Materials Transactions B-process Metallurgy And Materials Processing Science
ISSN:
1073-5615
Idioma:
Inglés
Tipo de recurso:
Artículo publicado
Clasificación temática:
Resumen
Ruthenium, as well as the rest of the platinum-group metals, is of crucial importance for industry due to its extraordinary catalytic activity and high-tech applications. Because of its scarcity and high value, there is an increasing interest towards its recovery from wastes. Chlorination metallurgy arises as one possible recovery method. The intrinsic kinetics of the chlorination of ruthenium oxide was studied with the aim of applying this process in a suitable recovery technology. Chlorination of RuO2 was investigated for temperatures between 973 K and 1073 K (700 °C and 800 °C) and chlorine partial pressure from 50 to 90 kPa. The reaction rate was measured by gravimetry and the rate equation was obtained. An activation energy of 259 ± 6 kJ mol−1 and a reaction order of 0.5 with respect of chlorine partial pressure were determined. The reaction product is unstable at atmospheric conditions. Formation of RuO2Cl2 is proposed based on experimental evidence; however, such product has not been confirmed yet.
Palabras clave:
Chlorination
,
Kinetics
,
Ruthenium Oxide
,
Ruthenium Tetroxide
,
Ruthenium Compound
Archivos asociados
Licencia
Identificadores
Colecciones
Articulos(CCT - PATAGONIA NORTE)
Articulos de CTRO.CIENTIFICO TECNOL.CONICET - PATAGONIA NORTE
Articulos de CTRO.CIENTIFICO TECNOL.CONICET - PATAGONIA NORTE
Citación
Guibaldo, Cristina Noemi; de Micco, Georgina; Bohe, Ana Ester; Intrinsic Kinetics of the Chlorination of RuO2 with Cl2 Between 973 K and 1073 K (700 °C and 800 °C); Springer; Metallurgical And Materials Transactions B-process Metallurgy And Materials Processing Science; 47; 2; 30-4-2016; 983-988
Compartir