Artículo
Rolling contact fatigue of ion nitrided and TiN coated AISI 4140 steel under pure rolling condition
Mandri, Alejo Daniel; Colombo, Diego Alejandro
; Sanchez, Nicolás Valentín; Brühl, Sonia Patricia; Dommarco, Ricardo


Fecha de publicación:
03/2025
Editorial:
Pergamon-Elsevier Science Ltd
Revista:
Engineering Failure Analysis
ISSN:
1350-6307
Idioma:
Inglés
Tipo de recurso:
Artículo publicado
Clasificación temática:
Resumen
This work studies the influence of the ion nitriding pre-treatment on the surface characteristics and, particularly, the rolling contact fatigue behavior of PVD TiN coated AISI 4140 steel. In addition, single ion nitriding and PVD TiN coating processes were also studied for comparative purposes. Depending on the substrate characteristics, the TiN coating remained practically intact throughout the test or delaminated after hundreds of thousands of load cycles, but it did not provide a measurable improvement on RCF life. Although the solely nitrided specimens did not have the expected influence as pre-treatment, they presented the best RCF performance, and it is attributed to the absence of interfaces and the hardening of the subsurface.
Palabras clave:
Ion nitriding
,
TiN coating
,
Duplex treatment
,
Rolling Contact Fatigue
Archivos asociados
Licencia
Identificadores
Colecciones
Articulos(CCT - SANTA FE)
Articulos de CTRO.CIENTIFICO TECNOL.CONICET - SANTA FE
Articulos de CTRO.CIENTIFICO TECNOL.CONICET - SANTA FE
Articulos(INTEMA)
Articulos de INST.DE INV.EN CIENCIA Y TECNOL.MATERIALES (I)
Articulos de INST.DE INV.EN CIENCIA Y TECNOL.MATERIALES (I)
Citación
Mandri, Alejo Daniel; Colombo, Diego Alejandro; Sanchez, Nicolás Valentín; Brühl, Sonia Patricia; Dommarco, Ricardo; Rolling contact fatigue of ion nitrided and TiN coated AISI 4140 steel under pure rolling condition; Pergamon-Elsevier Science Ltd; Engineering Failure Analysis; 170; 109311; 3-2025; 1-12
Compartir
Altmétricas